Alloy 625
Alloy 625 is a high‑strength, corrosion‑resistant nickel‑chromium‑molybdenum‑niobium superalloy known for exceptional performance from cryogenic temperatures up to 1800°F (982°C). Strength is derived from solid‑solution hardening by molybdenum and niobium, meaning no precipitation‑hardening heat treatment is required.
Standards & Designations
- UNS: N06625
- EN / W. Nr.: 2.4856
- AMS: 5599 (sheet/plate), 5666 (bars/forgings)
- ASTM/ASME: B443 (sheet/plate), B444 (tube/pipe), B446 (bars), B704/B705 (welded tube/pipe)
Corrosion resistance
Alloy 625 provides outstanding resistance to:
- Pitting & crevice corrosion due to high chromium & molybdenum
- Chloride stress‑corrosion cracking thanks to high nickel content
- Oxidizing & non‑oxidizing acids (nitric, phosphoric, sulfuric, hydrochloric)
- Seawater, brines, and contaminated marine environments
Heat treatment
Alloy 625 is typically supplied in the annealed condition.
- Solution annealing: ~2000°F (1093°C)
- No precipitation-hardening required (strength is inherent to the solid‑solution matrix).
Welding
- Machining: Alloy 625 is more difficult to machine than stainless steels due to its high strength and rapid work‑hardening behavior. Cutting tools must be rigidly supported, and machining should use slow speeds, heavy feeds, and sharp tooling to minimize work hardening. Carbide tooling is generally recommended.Although tough to machine, Alloy 625 maintains excellent corrosion resistance, even after significant cold work, which is common during machining operations.
- Forming: Alloy 625 offers excellent formability in both cold‑ and hot‑worked conditions. It is highly ductile, allowing deep drawing, bending, and cold‑rolling with minimal risk of cracking. Cold work significantly increases strength, so intermediate anneals may be required during heavy forming. Hot forming is typically followed by solution annealing to restore full corrosion resistance and mechanical performance.
- Welding: Alloy 625 has outstanding weldability, better than many other high‑alloy nickel materials. Welds resist intergranular corrosion, even in the as‑welded condition, and the alloy maintains resistance to chloride stress‑corrosion cracking. Common filler metals include ER625 (AMS 5837) for matching corrosion resistance. The alloy welds successfully with standard processes such as GTAW, GMAW, SMAW, and FCAW.
Typical applications
The list of applications for this general purpose grade is very extensive and includes:
- jet engine exhaust systems
- heat‑exchanger
- transfer piping
- reaction vessels
- furnace hardware
- distillation columns
- anti‑corrosion tubing & fasteners
- bellows, springs, subsea hardware
- seawater components
Chemical Composition (%)
| Grade | Cr | Ni | Mo | Nb + Ta | Fe | Mn | Si | C | Ti |
|---|---|---|---|---|---|---|---|---|---|
| 625 | 20.0 – 23.0 | Balance | 8.0 – 10.0 | 3.15 – 4.15 | 5.0 max | 0.5 max | 0.5 max | 0.1 max | 0.4 max |
Mechanical properties (annealed)
| Yield Strength .2% Offset (psi) | Ultimate Strength (psi) | Elongation in 2” (%) |
|---|---|---|
| 55,100 | 110,200 | 35 |
Other properties
| Specific Heat (BTU/lb-°F) | Electrical Resistivity at 68⁰F (μΩ-cm) | Thermal Conductivity (32–212°F) (BTU./ft.₂/hr./⁰F/ft) | Thermal Expansion 32⁰ – 212⁰F (In/In/⁰F×10‾⁶) |
|---|---|---|---|
| 0.098 | 126 | 112 | 9.0 × 10⁻⁶ |