321 / 321H
Type 321 is an austenitic stainless steel stabilized with titanium, designed to prevent carbide precipitation during exposure to temperatures in the 800–1500 °F range. This stabilization makes it highly resistant to intergranular corrosion, even after prolonged heating. It combines excellent oxidation resistance with good mechanical strength at elevated temperatures, making it suitable for high-temperature service in chemical, aerospace, and thermal processing industries
- 321: Standard grade with low carbon content (≤ 0.08%), optimized for resistance to sensitization and intergranular corrosion during welding or short-term high-temperature exposure.
- 321H: High-carbon variant (0.04–0.10%), specifically developed for improved creep strength and stress-rupture resistance during long-term service at temperatures above 1000 °F. This makes 321H the preferred choice for pressure vessels, furnace components, and other applications requiring durability under sustained high heat.
Corrosion resistance
321 and 321H stainless steels offer excellent resistance to intergranular corrosion due to titanium stabilization, which prevents carbide precipitation during exposure to temperatures in the 800–1500 °F range. This makes them suitable for environments where welded components or prolonged heating could otherwise lead to sensitization. Both grades also provide good resistance to general corrosion in mildly aggressive environments.
Heat resistance
These grades maintain outstanding oxidation resistance and mechanical strength at elevated temperatures. They can withstand intermittent service up to about 1650 °F (900 °C) and continuous service up to 1700 °F (925 °C). 321H, with its higher carbon content, delivers superior creep strength and stress-rupture resistance for long-term exposure above 1000 °F, making it ideal for high-temperature pressure vessels and furnace components.
Heat treatment
- Annealing/solution treatment: heat to 950–1120 °C (1750–2050 °F), then rapid cooling.
- Optionally, stabilizing heat treat at ~870–890 °C (1600–1630 °F) after solution treatment for enhanced grain stability.
Welding
Both 321 and 321H are readily weldable using standard austenitic stainless steel fillers. Grade 321 minimizes carbide precipitation during welding, making it suitable for welded structures, while 321H may require stabilization or post-weld heat treatment for critical high-temperature applications.
Typical applications
The list of applications for this general purpose grade is very extensive and includes:
- automotive/aircraft exhaust manifolds
- jet-engine parts
- heat exchangers
- expansion joints
- chemical processing
- refinery equipment
- high-temperature pressure vessels
- furnace components
AISI analysis (%)
| Grade | C | Mn | P | S | Si | Cr | Ni |
|---|---|---|---|---|---|---|---|
| 321 | .08 max | 2.0 max | .045 max | .030 max | .75 max | 17.0 to 19.0 | 9.0 to 12.0 |
| 321H | .04 – .10 | 2.0 max | .045 max | .030 max | .75 max | 17.0 to 19.0 | 9.0 to 12.0 |
Mechanical properties (annealed)
| Yield Strength .2% Offset (psi) | Ultimate Strength (psi) | Elongation in 2” (%) | Hardness (Rb) | Impact Charpy (ft. – lbs) | Elastic modulus (psi) |
|---|---|---|---|---|---|
| 30,000 | 75,000 | 40 | 85–95 | 122 | 28 × 10⁶ |
Other properties
| Creep Strength 1% Flow in 10,000 h at 1,000⁰F psi | Magnetic Permeability | Electrical Resistivity at 68⁰F (μΩ-cm) | Thermal Expansion 68⁰ – 212⁰F (In/In/⁰F×10‾⁶) | Thermal Conductivity (BTU./ft.₂/hr./⁰F/ft) |
|---|---|---|---|---|
| 12,500 | 1.02 | 29 | 9.28 × 10⁻⁶ | 8.8 (at 200⁰F) |