Duplex 2205
Grade 2205 is a duplex stainless steel with a mixed austenitic-ferritic microstructure, typically containing ~22% chromium, 5–6% nickel, and 3% molybdenum with nitrogen addition. It combines high mechanical strength with excellent corrosion resistance, particularly in chloride environments, making it a widely used alternative to 316 / 316L.
Standards & Designations
- UNS: S32205 / S31803
- EN / W. Nr.: 1.4462 / X2CrNiMoN22-5-3
- NACE: ISO 15156 / MR0175 compliant
- ASTM/ASME: A240 (plate), A276 (bars)
Corrosion resistance
Duplex Stainless Steel 2205 delivers excellent resistance to pitting, crevice corrosion, and stress corrosion cracking, significantly outperforming 304 and 316 grades. With a PREN value around 34–36, it is highly effective in chloride-containing environments such as seawater and chemical processing systems. It also provides strong resistance to organic and inorganic acids, particularly where chlorides are present.
Heat treatment
- Solution annealing: 1900–2050°F (1040–1120°C), followed by rapid cooling
- Maintains correct ferrite/austenite balance for optimal properties
- Cannot be hardened by heat treatment
- Cold working increases strength but may require re-annealing to restore ductility
Welding
- Machining: More difficult than austenitic grades due to higher strength; requires rigid tooling and controlled speeds.
- Forming: Higher forming forces are required compared to 316.
- Welding: Good weldability with controlled heat input; use ER2209/E2209
Typical applications
The list of applications for this general purpose grade is very extensive and includes:
- oil & gas (pipelines, separators)
- chemical processing equipment
- heat exchangers
- desalination plants
- pulp & paper industry
- marine and seawater handling components
- structural and industrial applications
Chemical Composition (%)
| Grade | C | Mn | Si | P | S | Cr | Ni | Mo | N |
|---|---|---|---|---|---|---|---|---|---|
| 2205 | .030 max | 2.0 max | 1.0 max | .030 max | .020 max | 21.0 to 23.0 | 4.5 to 6.5 | 2.5 to 3.5 | 0.14 to 0.20 |
Mechanical properties (annealed)
| Yield Strength .2% Offset (psi) | Ultimate Strength (psi) | Elongation in 2” (%) | Impact Charpy (ft. – lbs) | Elastic modulus (psi) |
|---|---|---|---|---|
| 65,000 – 80,000 | 90,000 – 116,000 | 20-25 | ~45 – 70 | 29.0×10⁶ |
Other properties
| Density (lb/in³) | Melting Range | Electrical Resistivity at 68⁰F (μΩ-cm) | Thermal Expansion 32⁰ – 212⁰F (In/In/⁰F×10‾⁶) |
|---|---|---|---|
| 0.278 | 2500–2640°F | 27-30 | 7.2-7.8 |